Superalloy Material A286 Gr660 GH2132 Heavy Hex Nut for Oil and Gas Refinery Projects Grade 4.8/6.8/8.8/10.9/12.9

NXF GROUP (New XiFei (SuZhou) Business Co.,Ltd)
Contact Now

Superalloy Material A286 Gr660 GH2132 Heavy Hex Nut for Oil and Gas Refinery Projects Grade 4.8/6.8/8.8/10.9/12.9

Finish : ZINC, Plain

Material : stainless steel

Place of Origin : Jiangsu, China

Brand Name : NXF

Standard : ANSI, A286 Gr660(GH2132)

Product name : Superalloy nut

Surface treatment : Customer's Request

Size : Customized Size

Grade : 4.8/6.8/8.8/10.9/12.9

Application : Industry

Color : Customized Colors

Head type : Hexaonal Head

Certificate : ISO

Packing : Carton

MOQ : 100 pieces

Price : $0.07/pieces 100-499 pieces

Contact Now

Product Description
Superalloy Material A286 Gr660 GH2132 Heavy Hex Nut for Oil and Gas Refinery Projects Grade 4.8/6.8/8.8/10.9/12.9
Superalloy Material A286 Gr660 GH2132 Heavy Hex Nut for Oil and Gas Refinery Projects Grade 4.8/6.8/8.8/10.9/12.9
Superalloy Material A286 Gr660 GH2132 Heavy Hex Nut for Oil and Gas Refinery Projects Grade 4.8/6.8/8.8/10.9/12.9
Specification
item
value
Finish
ZINC, Plain
Material
Stainless steel
Place of Origin
China
Jiangsu
Brand Name
NXF
Standard
ANSI
Product name
Superalloy nut
Standard
A286 Gr660(GH2132)
Surface treatment
Customer's Request
Size
Customized Size
Grade
4.8/6.8/8.8/10.9/12.9
Application
Industry
Color
Customized Colors
Head type
Hexaonal Head
Certificate
ISO
Packing
Carton
Packing & Delivery
Superalloy Material A286 Gr660 GH2132 Heavy Hex Nut for Oil and Gas Refinery Projects Grade 4.8/6.8/8.8/10.9/12.9
Superalloy Material A286 Gr660 GH2132 Heavy Hex Nut for Oil and Gas Refinery Projects Grade 4.8/6.8/8.8/10.9/12.9
To better ensure the safety of your goods, professional, environmentally friendly, convenient and efficient packaging services will be provided.
Company Profile
Superalloy Material A286 Gr660 GH2132 Heavy Hex Nut for Oil and Gas Refinery Projects Grade 4.8/6.8/8.8/10.9/12.9
Superalloy Material A286 Gr660 GH2132 Heavy Hex Nut for Oil and Gas Refinery Projects Grade 4.8/6.8/8.8/10.9/12.9
Superalloy Material A286 Gr660 GH2132 Heavy Hex Nut for Oil and Gas Refinery Projects Grade 4.8/6.8/8.8/10.9/12.9
Superalloy Material A286 Gr660 GH2132 Heavy Hex Nut for Oil and Gas Refinery Projects Grade 4.8/6.8/8.8/10.9/12.9
New XiFei (SuZhou) Business Co.,Ltd is one of the leading and most respected manufacturers in China. Our products include metals, machinery, containers, construction materials, mechanical products, electrical systems, and medical accessories. Established in 1980, XIFEI has been working diligently ever since to embrace the needs of our global customer base.We work to ensure absolute customer satisfaction. Our team has dedicated itself to perfecting our three core components, "Service, Management and Craftsmanship."
Certifications
Superalloy Material A286 Gr660 GH2132 Heavy Hex Nut for Oil and Gas Refinery Projects Grade 4.8/6.8/8.8/10.9/12.9
Superalloy Material A286 Gr660 GH2132 Heavy Hex Nut for Oil and Gas Refinery Projects Grade 4.8/6.8/8.8/10.9/12.9
FAQ
1. who are we?
We are based in Jiangsu, China, start from 2021,sell to South Asia(30.00%),Eastern Asia(10.00%),Mid East(10.00%),Eastern Europe(10.00%),South America(10.00%),Domestic Market(5.00%),North America(5.00%),Northern Europe(5.00%),Central America(5.00%),Africa(5.00%),Southeast Asia(5.00%). There are total about 101-200 people in our office.

2. how can we guarantee quality?
Always a pre-production sample before mass production;
Always final Inspection before shipment;

3.what can you buy from us?
Pipe,Flange,Steel plate,Pipe fittings,Alloy products

4. why should you buy from us not from other suppliers?
Wehave our own factories, quality can be controlled seriously. We Specialize in manufacturing about 21 years. We have professional testing department and testing equipment. We have 12 rich experience engineers & 20 senior technicians.

5. what services can we provide?
Accepted Delivery Terms: FOB,CFR,CIF,EXW,FCA;
Accepted Payment Currency:USD,EUR,CAD,HKD,CNY;
Accepted Payment Type: T/T,L/C,D/P D/A;
Language Spoken:English,Chinese

 Superalloy Material A286 Gr660 GH2132 Heavy Hex Nut for Oil and Gas Refinery Projects Grade 4.8/6.8/8.8/10.9/12.9 Manufactures

Superalloy Material A286 Gr660 GH2132 Heavy Hex Nut for Oil and Gas Refinery Projects Grade 4.8/6.8/8.8/10.9/12.9 Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: NXF GROUP (New XiFei (SuZhou) Business Co.,Ltd)
*Subject:
*Message:
Characters Remaining: (0/3000)